Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 90.0 kN/m | 514 pli | |
P & P Technology MS-N Nickel Graphite Conductive Adhesive P & P Technology conductive nickel/graphite adhesive is a one part electrically conductive room temperature curing elastomer. It is supplied as a readily extrudable paste that cures rapidly when exp.. |
|||
Tear Strength | 90.0 kN/m | 514 pli | Die C; ASTM D624 |
Covestro Texin® 5286 Thermoplastic Polyurethane, Polyether-based, Medical
(discontinued **) This grade is in chemical compliance with 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber articles intended for repeated use) subject to the limitations of this regulation and any other r.. |
|||
Tear Strength | 90.0 kN/m | 514 pli | Die C; ASTM D624 |
Covestro Texin® DP7-3008 Thermoplastic Polyurethane, Polyester-based, Aliphatic
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Tear Strength | 90.0 kN/m | 514 pli | ASTM D624 |
GRECO ISOTHANE 1090AE Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are Poly(adipate)ester based thermoplastic polyurethanes with good balanced qualities. They exhibit good toughness, abrasive resistance, solvent resistance, and transp.. |
|||
Tear Strength | 90.0 kN/m | 514 pli | ASTM D624 |
GRECO ISOTHANE 1180A Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tear Strength | 90.0 kN/m | 514 pli | ASTM D624 |
GRECO ISOTHANE 2090A Poly(caprolactone)ester TPUÂ Resin ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi.. |
|||
Tear Strength | 90.0 kN/m | 514 pli | MD; ISO 6383-2 |
Iran Petrochemical (PCC) 2404TC47 Low Density Polyethylene LDPE 2404TC47 Light duty FilmIt is used for very thin films requiring good optical properties for general packaging applications e.g. covering film with very low blocking tendency.Information provi.. |
|||
Tear Strength | 90.0 kN/m | 514 pli | MD; ISO 6383-2 |
Iran Petrochemical (PCC) 2602TH00 Low Density Polyethylene LDPE 2602TH00 high clarity film Applications: film, underblankets and films for medical applications.Information provided by Iran Petrochemical Commercial Co. |
|||
Tear Strength | 90.0 kN/m | 514 pli | ISO 34-1B |
Lubrizol Advanced Materials Pearlthane® 11T85 Polycaprolactone Copolyester based TPU Type : Pearlthane® 11T85 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Adequate hardness, excellent mechanical propert.. |
|||
Tear Strength | 90.0 kN/m | 514 pli | ISO 34B |
Huntsman AVALON® 85 AE Thermoplastic Polyurethane Introduction: AVALON 85 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 85 AE is part of the AVALON Perform Range and offers a premium soiling materi.. |
|||
Tear Strength | 90.0 kN/m | 514 pli | MD; ISO 6383-2 |
Iran Petrochemical (PCC) LT0470/KJ Low Density Polyethylene LT0470/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties. Application: stiffer thin films for textile p.. |
|||
Tear Strength | 90.0 kN/m | 514 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-1685AD Polyester Based TPU Stable melt viscosity, outstanding toughness & tear resistance, good workability for high frequency weldingInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 90.0 kN/m | 514 pli | DIN 53515 |
Lubrizol ESTANE® 58563 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 90.0 kN/m | 514 pli | ISO 34 |
Chengdu Polyster FH5550 Thermoplastic Polyether-ester Elastomer (TPEE) Blend of H5550 and self-made flame retardant material. Flame retardant, good balance of low and high temperature properties. Applications requiring flame retardancy, such as wires, cables and optica.. |
|||
Tear Strength | 90.0 kN/m | 514 pli | Die C; ASTM D624 |
Covestro Bayflex® XGT-50 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Tear Strength | 90.0 kN/m | 514 pli | normal; ISO 34-1 |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl.. |
|||
Tear Strength | 90.0 kN/m | 514 pli | DIN ISO 34-1/Bb |
BASF Elastollan B 90 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tear Strength | 90.1 kN/m | 514 pli | Die C; ASTM D412 |
Alliance Polymers Zythane™ 4090A Thermoplastic Polyurethane Elastomer Zythane™ 4090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tear Strength | 90.1 kN/m | 514 pli | Die C; ASTM D412 |
Alliance Polymers Zythane™ 5090A Thermoplastic Polyurethane Elastomer Zythane™ 5090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tear Strength | 90.1 kN/m | 514 pli | Die C; ASTM D412 |
Alliance Polymers Zythane™ 6075A Thermoplastic Polyurethane Elastomer Zythane™ 6075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tear Strength | 90.1 kN/m | 514 pli | Die C; ASTM D412 |
Alliance Polymers Zythane™ 7085AF Thermoplastic Polyurethane Elastomer Zythane™ 7085AF is a FR polyether-based TPU specifically formulated with non-halogenated flame retardants for extrusion applications with ease of processing. It exhibits excellent abrasion resistan.. |
|||
Tear Strength | >= 90.0 kN/m | >= 514 pli | ISO 34 |
Austin Novel Materials Texalan® 285A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tear Strength | >= 90.0 kN/m | >= 514 pli | ISO 34 |
Austin Novel Materials Texalan® 795A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |
|||
Tear Strength | 90.0 kN/m | 514 pli | ASTM D624 |
BASF Elastollan® 1180A Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Tear Strength | 90.0 kN/m | 514 pli | ASTM D624 |
BASF Elastollan® 685A15N Polyester Type Polyurethane Elastomer This grade is FDA compliant, section 177.2600 and 177.1680, for both wet and dry contact with food. The Elastollan 600 Series of products listed are products that are part of a new series of polyes.. |
|||
Tear Strength | 90.0 kN/m | 514 pli | ASTM D624 |
Wanhua Chemical Wanthane® WHT-1585 Polyester Based TPU Low cost, good mechanical properties, good processabilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tear Strength | 90.1 kN/m | 514 pli | Die C; ASTM D412 |
Alliance Polymers Zythane™ 7075A Thermoplastic Polyurethane Elastomer Zythane™ 7075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tear Strength | >= 90.0 kN/m | >= 514 pli | ISO 34 |
Austin Novel Materials Texalan® 798A PCL TPU Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech |