Lubrizol Advanced Materials PEARLCOAT® 161K Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlcoat®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLCOAT® 161K Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PEARLCOAT® 161K is a polyether based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low temperature flexibility and very good hydrolysis resistance. PEARLCOAT® 161K is used in melt coatings on textile substrates, for end-uses in industrial coatings (for life-jackets, etc.) obtained by extrusion and calendering.All information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 21.6 kg
10 g/10 min

@Load 47.6 lb
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
ASTM D2240
Tensile Strength, Yield 25.04 MPa
3632 psi
ASTM D412
Elongation at Break 650 %
650 %
ASTM D412
100% Modulus 0.00400 GPa
0.580 ksi
ASTM D412
300% Modulus 0.006998 GPa
1.015 ksi
ASTM D412
Tear Strength 70.1 kN/m
400 pli
ASTM D624 (Die C)
Abrasion 25
25
loss (mm³); DIN 53.516
Thermal Properties Metric English Comments
Melting Point 157 - 167 °C
314 - 332 °F
MQSA 111
Glass Transition Temp, Tg -43.9 °C
-47.0 °F
DSC, 10ºC/min; DIN 51.007
Processing Properties Metric English Comments
Zone 1 149 - 160 °C
300 - 320 °F
Zone 2 160 - 171 °C
320 - 340 °F
Zone 3 168 - 179 °C
335 - 355 °F
Zone 4 174 - 185 °C
345 - 365 °F
Die Temperature 174 - 185 °C
345 - 365 °F