Mechanical Properties Metric English Comments
Tear Strength 70.1 kN/m
400 pli
Die C, 51 mm/min; ASTM D624
PolyOne Geon™ Vinyl Flexible 90215 Polyvinyl Chloride, Flexible (PVC, Flexible)
Provisional Product Information - Physical and Mechanical properties based on initial production.Information provided by PolyOne
Tear Strength 70.1 kN/m
400 pli
Die C, 510 mm/min; ASTM D624
PolyOne Geon™ Vinyl Flexible A5DM0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne
Tear Strength 70.1 kN/m
400 pli
Die C, 510 mm/min; ASTM D624
PolyOne Geon™ Vinyl Flexible B8500 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tear Strength 70.1 kN/m
400 pli
Die C, 510 mm/min; ASTM D624
PolyOne Geon™ Vinyl Flexible B85B0 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tear Strength 70.1 kN/m
400 pli
Die C, 510 mm/min; ASTM D624
PolyOne Geon™ Vinyl Flexible C5D00 Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tear Strength 70.1 kN/m
400 pli
Die C, 510 mm/min; ASTM D624
PolyOne Geon™ Vinyl Flexible R264AE Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tear Strength 70.1 kN/m
400 pli
ASTM D624
Huntsman IROGRAN® A 65 P 4324 N TPU-Polyether
Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman
Tear Strength 70.1 kN/m
400 pli
Die C; ASTM D624
Mearthane Durethaneâ„¢ S DS-280A Solid Polyurethane Elastomer
TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..
Tear Strength 70.1 kN/m
400 pli
ASTM D624
ITW Devcon Flexane® Rubber Repair / Castable Urethane Brushable, Black
Information provided by ITW Devcon
Tear Strength 70.1 kN/m
400 pli
ASTM D624 (Die C)
Lubrizol Advanced Materials PEARLCOAT® 161K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 161K is a polyether based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low temperature flexibility and very good hydrolysis resistance..
Tear Strength 70.1 kN/m
400 pli
ASTM D624 DIE C
Lubrizol Advanced Materials Pearlthane® 12C75 Thermoplastic Polyurethane Elastomer
Pearlthane® 12C75 is a standard polyester based TPU supplied in form of translucent, colorless pellets, specially designed for compounds in which TPU is used as an additive. Features include low ..
Tear Strength 70.1 kN/m
400 pli
ASTM D624
ITW Devcon Flexane® Rubber Repair / Castable Urethane High Performance Putty, Black
Information provided by ITW Devcon
Tear Strength 70.1 kN/m
400 pli
ASTM D624
Multibase Multi-Flex® A 9002 MR TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good ..
Tear Strength 70.1 kN/m
400 pli
Initial Tear Strength
Saint-Gobain CHR® SG03-14(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Tear Strength 70.1 kN/m
400 pli
Initial Tear Strength
Saint-Gobain CHR® SG05-14(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Tear Strength 70.1 kN/m
400 pli
Initial Tear Strength
Saint-Gobain CHR® SG06-14(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Tear Strength 70.1 kN/m
400 pli
Initial Tear Strength
Saint-Gobain CHR® SG13-14(R) High Performance Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Tear Strength 70.1 kN/m
400 pli
Initial Tear Strength
Saint-Gobain CHR® SG15-14(R) High Performance Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Tear Strength 70.1 kN/m
400 pli
Initial Tear Strength
Saint-Gobain CHR® SG16-14(R) High Performance Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Tear Strength 70.1 kN/m
400 pli
Warp/Longitudinal direction; ASTM D1000
Saint-Gobain COHRlastic® 3032 Low Temperature Flexibility Silicone Coated Fabric
Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi..
Tear Strength 70.1 kN/m
400 pli
Tensile Strength (Warp)
Saint-Gobain Chemfab® q-GUARD® 18 Insulation Jacketing
Description: q-GUARD® is a thermally durable and fire-safe composite developed specifically for use with removable and reusable insulation systems. Based upon PTFE fluorocarbon resins and fibergl..
Tear Strength 70.1 kN/m
400 pli
Tensile Strength (Warp)
Saint-Gobain Chemfab® TCK® 1590 High-Strength Leno Weave Open Mesh Belting Material
Description: General Notes on Saint Gobain Chemfab® TCK® Open Mesh Belting Products:TCK belting products are PTFE (PTFE = polytetrafluoroethylene) coated Kevlar®, a high-temperature aramid ..
Tear Strength 70.1 kN/m
400 pli
Saint-Gobain COHRlastic® CF4444 Reversion Resistant Reinforced Solid Rubber
Description: COHRlastic® CF silicone solid rubber reinforced with fiberglass is a dimensionally-stable, durable material for press pads, belting and gasketing. It is available in six construction..
Tear Strength 70.1 kN/m
400 pli
Tensile Strength (Fill)
Saint-Gobain Chemfab® TCK® 1000 High-Strength Leno Weave Open Mesh Belting Material
Description: General Notes on Saint Gobain Chemfab® TCK® Open Mesh Belting Products:TCK belting products are PTFE (PTFE = polytetrafluoroethylene) coated Kevlar®, a high-temperature aramid ..
Tear Strength 70.1 kN/m
400 pli
ASTM D624
Teknor Apex Uniprene® UN-2467A Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex..