Westlake Tymax™ GT7058 Anhydride Modified Acrylate Copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , Anhydride-Modified Polyethylene
Manufacturer Westlake Chemical Corporation
Trade Name Tymax™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Tymax™ GT7058 Anhydride Modified Acrylate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Westlake GT7058 is an anhydride modified acrylate copolymer designed for blown film extrusion that contains no slip and no antiblock additives. This resin is designed to function as a coextruded tie layer in multilayer film applications. Westlake GT7058 is designed to tie polyethylene to resins that typically have poor bonding characteristics such as polyamide and EVOH. Its applications include: blown film, packaging, and tie-layer.
Physical Properties Metric English Comments
Density 0.943 g/cc
0.0341 lb/in³
ASTM D4883
Methyl Acrylate Content 24 %
24 %
Westlake
Melt Flow 2.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 74.0 °C
165 °F
DSC; ASTM D3418
Crystallization Temperature 43.0 °C
109 °F
DSC; ASTM D3418