Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 25.04 MPa | 3632 psi | ASTM D412 |
Lubrizol Advanced Materials PEARLCOAT® 161K Thermoplastic Polyurethane Elastomer PEARLCOAT® 161K is a polyether based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low temperature flexibility and very good hydrolysis resistance.. |