Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 167 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 166 - 167 °C
331 - 333 °F
Average value: 166 °C Grade Count:5
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
Melting Point 164 - 167 °C
327 - 333 °F
ASTM D3418
Solvay Specialty Polymers Hylar® 5000 HG Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Hylar® 5000 HG is a crystalline high molecular weight powder form of polyvinylidene fluoride specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically strong..
Melting Point 156 - 167 °C
313 - 333 °F
Huntsman/TMA
Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade
Introduction: IROGRAN A 78 E 4723 is a thermoplastic polyester- polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and high mec..
Melting Point 120 - 167 °C
248 - 333 °F
Indium Corp. Indalloy 98 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Melting Point 154 - 167 °C
309 - 333 °F
Indium Corp. Indalloy® 9 Sn-Pb-In Solder Alloy
General purpose solder in 160° C range with good physical properties.Information provided by the manufacturer, Indium Corporation.
Melting Point 157 - 167 °C
314 - 332 °F
MQSA 111
Lubrizol Advanced Materials PEARLCOAT® 161K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 161K is a polyether based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low temperature flexibility and very good hydrolysis resistance..
Melting Point 164 - 167 °C
327 - 333 °F
DSC
Solvay Specialty Polymers Hylar® 5000 HG Polyvinylidene Fluoride (PVDF)
Hylar® 5000 HG is a crystalline high molecular weight powder form of polyvinylidene fluoride (PVDF) specifically designed for solvent-based coatings to provide improved gloss. It forms mechanical..
Melting Point 163 - 167 °C
325 - 333 °F
DSC; ISO 3146
Borealis HC207TF Polypropylene Homopolymer
HC207TF is a special nucleated polypropylene homopolymer intended for thermoforming packaging. Applications: HC207TF is recommended for in-line and off line thermoforming, high transparent trays, c..
Melting Point 162 - 167 °C
324 - 333 °F
Addcomp PRIEX® Ionomer 42101 PP homopolymer
Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t..
Melting Point 164 - 167 °C
327 - 333 °F
10°C/min.; ISO 3146
Azoty Tarnow™ TARNOFORM 500 HI4 POM
Easy flow high impact grade, possessing also high damping capacityInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Melting Point 162 - 167 °C
324 - 333 °F
Addcomp PRIEX® Ionomer 40101 PP homopolymer
Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t..
Melting Point 162 - 167 °C
324 - 333 °F
Average value: 166 °C Grade Count:11
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
Melting Point 162 - 167 °C
324 - 333 °F
Average value: 166 °C Grade Count:11
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..
Melting Point 160 - 167 °C
320 - 333 °F
Average value: 164 °C Grade Count:18
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..
Copyright © lookpolymers.com All Rights Reserved