Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -43.9 °C | -47.0 °F | DSC, 10ºC/min; DIN 51.007 |
Lubrizol Advanced Materials PEARLCOAT® 161K Thermoplastic Polyurethane Elastomer PEARLCOAT® 161K is a polyether based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low temperature flexibility and very good hydrolysis resistance.. |