Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Zone 2 = 320 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 160 °C
320 °F
Termopol Termoton® K2GA5050A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
Zone 2 160 °C
320 °F
Termopol Termoton® K6GA4040A TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
Zone 2 160 - 190 °C
320 - 374 °F
Lubrizol Advanced Materials PEARLTHANE® 12K85A Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 12K85A is a standard polyester-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be e..
Zone 2 160 - 190 °C
320 - 374 °F
Lubrizol Advanced Materials PEARLTHANE® 12K92A Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 12K92A is a standard polyester-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be e..
Zone 2 160 - 191 °C
320 - 375 °F
Lubrizol Advanced Materials PEARLTHANE® 12K85LB Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 12K85 LB is a standard polyester-based TPU with a lubricating additive, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mech..
Zone 2 160 - 170 °C
320 - 338 °F
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLCOAT® 126K is a polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and medium softening point. PEARLCOAT® 1..
Zone 2 160 - 170 °C
320 - 338 °F
Injection Molding
Kolon ELLAS K-395F Ether Based Thermoplastic Polyurethane
ApplicationsExtrusionHighly Pressurized Hose Information provided by API-Kolon.
Zone 2 160 - 170 °C
320 - 338 °F
Extrusion Molding
Kolon ELLAS K-785A Ester Based Thermoplastic Polyurethane
ApplicationsCompoundingFilm/SeatT-DIE High Frequency FilmPVC/Rubber Compound Information provided by API-Kolon.
Zone 2 160 - 170 °C
320 - 338 °F
Lubrizol Advanced Materials PEARLCOAT® 127K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 127K is a polyester based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low-temperature flexibility and medium softening point. PEARLCOATÂ..
Zone 2 160 - 171 °C
320 - 340 °F
Lubrizol Advanced Materials PEARLCOAT® 161K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 161K is a polyether based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low temperature flexibility and very good hydrolysis resistance..
Zone 2 160 - 170 °C
320 - 338 °F
Lubrizol Advanced Materials PEARLCOAT® 125K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 125K is a polyester based TPU, supplied in form of translucent, colorless pellets, featuring medium softening point, and consistent quality pellets, low gel content as well low-tempera..
Zone 2 160 - 171 °C
320 - 340 °F
Lubrizol Advanced Materials PEARLCOAT® 163K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 163K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE..
Zone 2 160 - 171 °C
320 - 340 °F
Lubrizol Advanced Materials PEARLCOAT® 165K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 165K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low-temperature flexibility and very good hydrolysis resistance. PE..
Zone 2 160 - 170 °C
320 - 338 °F
Lubrizol Advanced Materials PEARLCOAT® 168K Thermoplastic Polyurethane Elastomer
PEARLCOAT® 168K is a polyether-based TPU, supplied in form of translucent, colorless pellets, offering adequate hardness, excellent low-temperature flexibility and very good hydrolysis resistance..
Zone 2 160 °C
320 °F
Borealis Borcell™ HE1123 High Density Polyethylene
Borcell™ HE1123 is a high density polyethylene compound intended for the insulation of radio frequency coaxial cables. Borcell™ HE1123 is designed to give the lowest possible cable attenuation by..
Zone 2 160 °C
320 °F
Lubrizol Estane® ALR G500 Water Absorbent Thermoplastic Polyurethane
Type: Estane® ALR G500 is an aliphatic thermoplastic polyurethane (TPU) resin designed to absorb water and transport moisture.Features: Contains UV additivesAvailable in AmericasInformation Provide..
Zone 2 160 °C
320 °F
Blown Film Coextrusion
DuPont™ Appeel® 72D799 Sealing Resin
DuPont™ Appeel® 72D799 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDP..
Zone 2 160 °C
320 °F
Blown Film Coextrusion
DuPont™ Appeel® 72D811 Sealing Resin
DuPont™ Appeel® 72D811 resin is designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDPE, LDPE, EVA, and Ion..
Zone 2 160 °C
320 °F
Cast Film/Sheet Processing
DuPont™ Appeel® 72D811 Sealing Resin
DuPont™ Appeel® 72D811 resin is designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDPE, LDPE, EVA, and Ion..
Zone 2 160 °C
320 °F
Blown Film Coextrusion
DuPont™ Bynel® 30E753 Anhydride Modified Ethylene Vinyl Acetate
BYNEL® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Zone 2 160 °C
320 °F
Blown Film Extrusion
DuPont™ Elvaloy® AC 1330 Ethylene Methyl Acrylate
Elvaloy® AC 1330 is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® A..
Zone 2 160 °C
320 °F
Extrusion Coating
DuPont™ Elvaloy® AC34035 Ethylene Methyl Acrylate
Elvaloy® AC 34035 is a copolymer of ethylene and butyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy® A..
Zone 2 160 °C
320 °F
Blown Film Coextrusion
DuPont™ Elvax® 3128-1 Ethylene Vinyl Acetate
DuPont™ Elvax® 3128-1 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® ..
Zone 2 160 °C
320 °F
Blown Film Coextrusion
DuPont™ Nucrel® 30705 Ethylene Acrylic Acid
Nucrel® 30705 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethyle..
Zone 2 160 °C
320 °F
Blown Film Coextrusion
DuPont™ Surlyn® E185SB Ionomer Resin
Surlyn® E185SB is an ionomer of an acid copolymer resin. It is designed for coextrusion with high-density polyethylene in peelable seals applications. It can be used in extrusion equipment designed..
Zone 2 160 °C
320 °F
Cast Film/Sheet Processing
DuPont™ Surlyn® E185SB Ionomer Resin
Surlyn® E185SB is an ionomer of an acid copolymer resin. It is designed for coextrusion with high-density polyethylene in peelable seals applications. It can be used in extrusion equipment designed..
Zone 2 160 °C
320 °F
Blown Film Coextrusion
DuPont™ Surlyn® 1706 Zinc Ionomer
Surlyn® 1706 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t..
Zone 2 160 °C
320 °F
Blown Film Coextrusion
DuPont™ Surlyn® 1707 Sodium Ionomer
Surlyn® 1707 is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer t..
Zone 2 160 °C
320 °F
Blown Film Coextrusion
DuPont™ Surlyn® 1825 Zinc Ionomer
Surlyn® 1825 is available for use in conventional blown, cast film, sheet extrusion and coextrusion equipment designed to process polyethylene and ethylene copolymer type resins. SURLYN® 1825 comp..
Zone 2 160 °C
320 °F
Blown Film Coextrusion
DuPont™ Surlyn® 2601B Sodium Ionomer
Surlyn® 2601B is available for use in conventional blown, cast film, and sheet extrusion equipment. It is also used in coextrusion equipment designed to process polyethylene and ethylene copolymer ..