Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loxim 831 02T HB Polypropylene Compound, 30% Talc Filled, Flame Retardant

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Talc Filler , Polypropylene, Flame Retardant
Manufacturer Loxim Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loxim 831 02T HB Polypropylene Compound, 30% Talc Filled, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.05 - 1.15 g/cc
1.05 - 1.15 g/cc
ASTM D792
Filler Content 30 %
30 %
Linear Mold Shrinkage 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 24.0 - 26.0 MPa
3480 - 3770 psi
ASTM D683
Flexural Modulus 2.20 - 2.40 GPa
319 - 348 ksi
ASTM D790
Izod Impact, Notched 0.400 - 0.600 J/cm
0.749 - 1.12 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 - 115 °C
230 - 239 °F
ASTM D1525, HDT Method B
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Users viewing this material also viewed the following: