Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 90.0 - 115 °C | 194 - 239 °F | |
Reliance Industries Polypropylene Impact Copolymer Typical properties of Reliance - Repol Polypropylene grades. Properties depend on rubber content, presence of nucleating agent, MFIInformation provided by Reliance Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 - 115 °C | 230 - 239 °F | ASTM D1525, HDT Method B |
Loxim 830 02C HB Polypropylene Compound, 30% Calcite Filled, Flame Retardant Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 - 115 °C | 230 - 239 °F | ASTM D1525, HDT Method B |
Loxim 830 02T V0 Polypropylene Compound, 30% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 110 - 115 °C | 230 - 239 °F | ASTM D1525, HDT Method B |
Loxim 831 02T HB Polypropylene Compound, 30% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 113 - 115 °C | 235 - 239 °F | Average value: 114 °C Grade Count:3 |
Overview of materials for Acrylic, Cast This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |