Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.15 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.00 - 1.15 g/cc
1.00 - 1.15 g/cc
Michelman® Hydrosize® HP-1632 Polyimide solution
Polyimide solutionHydrosize® HP-1632 is a specialty coating and high temperature fiber sizing with excellent adhesion properties and abrasion resistance.Information provided by Michelman®
Specific Gravity 1.05 - 1.15 g/cc
1.05 - 1.15 g/cc
Michelman® Hydrosize® U1-03 Phenoxy modified polyurethane dispersion
Description: Phenoxy modified polyurethane dispersionUsage: Hydrosize® U1-03 is designed to be a fiber sizing coating with excellent adhesion and abrasion resistanceInformation provided by Michel..
Specific Gravity 1.00 - 1.15 g/cc
1.00 - 1.15 g/cc
Michelman® Hydrosize® U2-01 Nonionic polyurethane emulsion
Description: Nonionic polyurethane emulsionUsage: Hydrosize® U2-01 is a high strength sizing for glass and carbon chopped fiber with excellent adhesion.Information provided by Michelman®
Specific Gravity 1.00 - 1.15 g/cc
1.00 - 1.15 g/cc
Michelman® Hydrosize® U2022 Nonionic polyurethane emulsion
Description: Nonionic polyurethane emulsionUsage: Hydrosize® U2022 is an APE free, high strength sizing for glass and carbon chopped fiber, with excellent adhesion.Information provided by Michelm..
Specific Gravity 1.00 - 1.15 g/cc
1.00 - 1.15 g/cc
Michelman® Hydrosize® U5-01 Polyurethane dispersion
Description: Polyurethane dispersionUsage: Hydrosize® U5-01 is a specialty coating and fiber sizing which offers improved thermal stability, higher strength and elongation to breakInformation pro..
Specific Gravity 1.00 - 1.15 g/cc
1.00 - 1.15 g/cc
Michelman® Hydrosize® U6-01 Polyurethane solution
Description: Polyurethane solutionUsage: Hydrosize® U6-01 is an aqueous polyurethane solution designed to be used as a fiber sizing agent for continuous nylon and epoxy reinforcements.Information..
Specific Gravity 1.00 - 1.15 g/cc
1.00 - 1.15 g/cc
Michelman® Hydrosize® U7-01 Polyurethane dispersion
Description: Polyurethane dispersionUsage: Hydrosize® U7-01 is a specialty coating and fiber sizing.Information provided by Michelman®
Specific Gravity 1.00 - 1.15 g/cc
1.00 - 1.15 g/cc
Michelman® Hydrosize® U8-01 Nonionic polyurethane dispersion
Description: Nonionic polyurethane dispersionUsage: Hydrosize® U8-01 is an APE free sizing for chopped glass and carbon fiber.Application data: Soft, polyether based polyurethane sizing with exce..
Specific Gravity 1.10 - 1.15 g/cc
1.10 - 1.15 g/cc
Michelman® Michem® Coat 82 Water resistance coating
Description: Water resistance coating with intermediate moisture barrier and higher COF.Usage: Michem® Coat 82 is a repulpable, printable, and cold set gluable coating optimized for water resista..
Specific Gravity 1.05 - 1.15 g/cc
1.05 - 1.15 g/cc
Michelman® Michem® Emulsion 48440 Polymer solution
Description: Polymer solutionUsage: Michem® Emulsion 48440 is used for fiber sizing.We serve many markets through Michem® Emulsion, including: paint & coatings; fiberglass; inks and overprint ..
Specific Gravity 1.12 - 1.15 g/cc
1.12 - 1.15 g/cc
ASTM D792
Loxim 500 00HB Polycarbonate/Acrylonitrile Butadiene Styrene
Information provided by Loxim Industries
Specific Gravity 1.05 - 1.15 g/cc
1.05 - 1.15 g/cc
ASTM D792
Loxim 820 02T V0 Polypropylene Compound, 20% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Specific Gravity 1.05 - 1.15 g/cc
1.05 - 1.15 g/cc
ASTM D792
Loxim 830 01 HBCC Polypropylene Compound 30% Chemically Coupled, Flame Retardant
Information provided by Loxim Industries
Specific Gravity 1.05 - 1.15 g/cc
1.05 - 1.15 g/cc
ASTM D792
Loxim 830 02C HB Polypropylene Compound, 30% Calcite Filled, Flame Retardant
Information provided by Loxim Industries
Specific Gravity 1.05 - 1.15 g/cc
1.05 - 1.15 g/cc
ASTM D792
Loxim 830 02T HB Polypropylene Compound, 30% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Specific Gravity 1.05 - 1.15 g/cc
1.05 - 1.15 g/cc
ASTM D792
Loxim 830 12 HB Polypropylene Compound, Flame Retardant
Information provided by Loxim Industries
Specific Gravity 1.05 - 1.15 g/cc
1.05 - 1.15 g/cc
ASTM D792
Loxim 831 02T HB Polypropylene Compound, 30% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Specific Gravity 1.00 - 1.15 g/cc
1.00 - 1.15 g/cc
Michelman® Hydrosize® U1-01 Nonionic polyurethane dispersion
Description: Nonionic polyurethane dispersionUsage: Hydrosize® U1-01 is a sizing for chopped glass and carbon fiber with excellent adhesion and good color and pH stability.Application data: Soft,..
Specific Gravity 1.14 - 1.15 g/cc
1.14 - 1.15 g/cc
ASTM D792
Ensinger TECAST™ Cast Nylon (PA)
TECAST™ Cast Nylon reduces downtime in heavy equipment applications. It is a low cost alternative for many non-ferrous machined parts. It has self-lubricating qualities which provide for excellen..
Specific Gravity 1.05 - 1.15 g/cc
1.05 - 1.15 g/cc
IEC 1212-2 7.2
Hippe PF CP 22 Cellulose Paper Reinforced Phenolic Resin - Round, Rolled Tube
High-voltage, electrical applications at power frequencies. High electric strength in oil.Information provided by Hippe.
Specific Gravity 1.11 - 1.15 g/cc
1.11 - 1.15 g/cc
ASTM D792
Buckeye Polymers BP RPP 3005 GR BLK Polypropylene, Glass Filled
Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en..
Specific Gravity 1.11 - 1.15 g/cc
1.11 - 1.15 g/cc
ASTM D792
Buckeye Polymers BP RPP 3009 GK3 BLK Polypropylene, Glass Filled
Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en..
Specific Gravity 1.11 - 1.15 g/cc
1.11 - 1.15 g/cc
ASTM D792
Buckeye Polymers BP RPP 3009 GKW Polypropylene, Glass Filled
Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en..
Specific Gravity 1.11 - 1.15 g/cc
1.11 - 1.15 g/cc
ASTM D792
Buckeye Polymers BP RPP 3009 GK BLK Polypropylene, Glass Filled
Product Information: Our glass reinforced product lines exhibit increased tensile strength, stiffness, and heat deflection. Highly optimized glass reinforced PP resins have successfully replaced en..
Specific Gravity 1.05 - 1.15 g/cc
1.05 - 1.15 g/cc
ASTM D792
Loxim 830 01 HB Polypropylene Compound, Flame Retardant
Information provided by Loxim Industries
Copyright © lookpolymers.com All Rights Reserved