Polymer Property : Flexural Modulus = 348 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.15 - 2.40 GPa
312 - 348 ksi
ASTM D790
Prodways PLASTCure Model 300 3D Printing Polymer
Good mechanical properties.Broad range of dental model applications.Information provided by Genistar.
Flexural Modulus 2.10 - 2.40 GPa
305 - 348 ksi
ASTM D790-04
Proto3000 Objet Digital Materials™ DM_7230 Transparent Prototyping Polymer
Primary material: FullCure720Secondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide ..
Flexural Modulus 2.30 - 2.40 GPa

@Temperature -20.0 - -20.0 °C
334 - 348 ksi

@Temperature -4.00 - -4.00 °F
Average value: 2.32 GPa Grade Count:5
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Flexural Modulus 2.00 - 2.40 GPa
290 - 348 ksi
ASTM D790
Huntsman RenShape® SL 7820 Stereolithography Plastic
RenShape® SL 7820 stereolithography material is a white, low viscosity and stable liquid that produces strong black models and prototypes with good surface fi nish and detail, and ABS-like appear..
Flexural Modulus 2.20 - 2.40 GPa
319 - 348 ksi
ASTM D790
Loxim 600 00HB Polycarbonate/Polybutylene Terephthalate
Information provided by Loxim Industries
Flexural Modulus 2.20 - 2.40 GPa
319 - 348 ksi
ASTM D790
Loxim 831 02T HB Polypropylene Compound, 30% Talc Filled, Flame Retardant
Information provided by Loxim Industries