Loctite® 3180 Deep Potting Polyurethane

Category Polymer , Adhesive , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Adhesive
Manufacturer Loctite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® 3180 Deep Potting Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PottersLoctite® Potting materials are used on electronic device housings to enhance mechanical strength, provide electrical insulation and enhance vibration and shock resistance of assemblies. For electronics assembly, Loctite offers deep potting, high adhesion, non-corrosive, and thermally conductive potting products. These can be cured with heat, UV light, or moisture.Loctite® 3180 Deep Potting PolyurethaneA re-enterable polyurethane for deep potting applications that require flexibility, impact strength and repairability. Cure Type: Heat Bonding Type: 2 part polyurethane
Physical Properties Metric English Comments
Viscosity 1000 cP
1000 cP
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore A 10
10
Hardness, Shore OO 65
65
Thermal Properties Metric English Comments
CTE, linear 377 µm/m-°C

@Temperature 20.0 °C
209 µin/in-°F

@Temperature 68.0 °F
Glass Transition Temp, Tg -83.0 °C
-117 °F
Processing Properties Metric English Comments
Cure Time 5.00 min

@Temperature 85.0 °C
0.0833 hour

@Temperature 185 °F
960 min

@Temperature 23.0 °C
16.0 hour

@Temperature 73.4 °F
Pot Life 10.0 min

@Temperature 23.0 °C
10.0 min

@Temperature 73.4 °F
Gel Time 720 min
720 min