Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -83.0 - 71.0 °C | -117 - 160 °F | Average value: -34.4 °C Grade Count:34 |
Overview of materials for Thermoset Polyurethane, Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values .. |
|||
Glass Transition Temp, Tg | -83.0 °C | -117 °F | |
Loctite® 3171 Deep Potting Polyurethane PottersLoctite® Potting materials are used on electronic device housings to enhance mechanical strength, provide electrical insulation and enhance vibration and shock resistance of assemblies.For e.. |
|||
Glass Transition Temp, Tg | -83.0 °C | -117 °F | |
Loctite® 3180 Deep Potting Polyurethane PottersLoctite® Potting materials are used on electronic device housings to enhance mechanical strength, provide electrical insulation and enhance vibration and shock resistance of assemblies. For .. |