Indium Corp. Indalloy 35 Bismuth Solder Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 35 Bismuth Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 10.11 g/cc
0.3652 lb/in³
Thermal Properties Metric English Comments
Melting Point 73.0 - 93.0 °C
163 - 199 °F
Solidus 73.0 °C
163 °F
Liquidus 93.0 °C
199 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 50 %
50 %
Cadmium, Cd 7.0 %
7.0 %
Lead, Pb 39 %
39 %
Tin, Sn 4.0 %
4.0 %