Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1000 cP @Temperature 25.0 °C |
1000 cP @Temperature 77.0 °F |
Uncured |
Permabond HM162 Anaerobic Retainer Permabond® HM162 is a medium viscosity retaining compound that cures when confined between metal parts to form an extremely tough bond. It is best suited for cylindrical parts and where high temper.. |
|||
Viscosity | 1000 cP | 1000 cP | |
Resinlab® CYNERGY CA6104 Adhesive Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates.. |
|||
Viscosity | 1000 - 2000 cP @Temperature 25.0 °C |
1000 - 2000 cP @Temperature 77.0 °F |
Uncured |
Permabond UV7141 UV-curable Adhesive Permabond UV7141 is a UV-curable adhesive with a secondary anaerobic cure mechanism. This makes it ideal for bonding materials such as ceramic-coated glass, mirrors, etc. where UV-light cannot penet.. |
|||
Viscosity | 1000 cP | 1000 cP | Part B, RVT, #2, 2.5 rpm; TM R050-12 |
Resinlab® EP1385 Clear Epoxy Formulation Resinlab™ EP1385 Clear is an epoxy formulation designed for applications requiring resistance to E-85 type fuels. It has good wetting and adhesion to most surfaces. It has very good resistance to w.. |
|||
Viscosity | 1000 cP | 1000 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1171 P (SIBS) Linear Triblock Copolymer Description: Kraton D1171 P is a clear, linear triblock copolymer based on styrene, butadiene and isoprene with a polystyrene content of 19%. It is supplied from North America in the form: Kraton D1.. |
|||
Viscosity | 1000 - 1500 cP | 1000 - 1500 cP | |
Huntsman Tactix 556 Epoxy Weight per Epoxide (EEW, g/eq) 215 to 235.Comments/Applications: Dicyclopentadiene based epoxy. Very low moisture pickup. Suggested for adhesives and composites used at elevated temperatures in a .. |
|||
Viscosity | 1000 - 1500 cP | 1000 - 1500 cP | |
Huntsman Tactix 556 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 215 to 235.Comments/Applications: Dicyclopentadiene based epoxy. Very low moisture pickup. Suggested for adhesives and composites used at elevated temperatures in a .. |
|||
Viscosity | 1000 - 1200 cP | 1000 - 1200 cP | B component |
Taiwan PU Corporation TPL-THANE 5085-A/B High Pressure Urethane Spraying Elastomer 5085-A is a high reactivity polyethamine content extender. 5085-B is a methylene diphenyklene dissocyanate(MDI). They make up the third generation high pressure urethane spraying elastomer. It ha.. |
|||
Viscosity | 1000 - 1400 cP | 1000 - 1400 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-737 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Non-yellowing, aliphatic gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for.. |
|||
Viscosity | 1000 cP | 1000 cP | 1.4% NaCl added |
Solvay MACKADET® SBC--8 Surfactant Product Description: Mackadet SBC-8 is a concentrated blend of mild surfactants for use as a base for high foaming surfactant systems. Mackadet SBC-8 responds rapidly to viscosity building with the .. |
|||
Viscosity | 1000 cP | 1000 cP | Mixed (cp #40, 10 rpm) |
Tra-Con Tra-Bond 546S01 Low Viscosity UV Curable Adhesive TRA-BOND 546S01 is a low viscosity UV curable adhesive with a secondary heat curing system to achieve a high Tg. It exhibits excellent adhesion to glass and many other substrates, making it ideal fo.. |
|||
Viscosity | 1000 cP | 1000 cP | at 20 RPM |
Loctite® 312 Acrylic Bonding Adhesive Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. .. |
|||
Viscosity | 1000 - 3000 cP | 1000 - 3000 cP | Solution 15% in MEK |
Wanhua Chemical Wanthane® WHT-6420B TPU Solvent-Based Adhesive Wide viscosity range, high crystallization rate, low activation temperature, good solvent solubility, accurate control of viscosity, outstanding bonding strength for PVC, polyamide, polyester, PU, c.. |
|||
Viscosity | 1000 - 10000 cP | 1000 - 10000 cP | Unmilled Cement; Zeon Test #328 |
Zeon Chemicals Nipol® 1001LG Nitrile Elastomer Nipol 1001LG is a copolymer of butadiene and acrylonitrile with very high oil resistance. Its properties are similar to those of Nipol 1001CG with the exception that: a) nomilling is required for un.. |
|||
Viscosity | 1000 cP | 1000 cP | dynamic |
Dow Corning SYL-OFF® SL 80 RELEASE MODIFIER Maleate-inhibited release modifier, thin film, high efficiency, medium viscosity, excellent bath stabilityInformation provided by Dow Corning |
|||
Viscosity | 1000 - 3000 cP @Temperature 23.0 °C |
1000 - 3000 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 320NC Optically Opaque Epoxy Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Viscosity | 1000 - 3000 cP | 1000 - 3000 cP | dynamic |
Dow Corning 2-2078 FLUID A liquid amino phenyl silicone resin primarily for use in hair care products, but has utility in color cosmetics as well.Information provided by Dow Corning |
|||
Viscosity | 1000 - 2000 cP @Temperature 25.0 °C |
1000 - 2000 cP @Temperature 77.0 °F |
MA143LFE |
C.O.I.M. FILCO® 358 Film Former for Glass Fiber Sizes Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar.. |
|||
Viscosity | 1000 cP | 1000 cP | Mixed |
Armstrong C-1/E Epoxy Adhesive A versatile, low viscosity, unfilled resin used for electrical potting and laminating applications. It is an excellent insulator, and provides outstanding chemical resistance to most compoundsInfor.. |
|||
Viscosity | 1000 - 1700 cP | 1000 - 1700 cP | |
3M Pronto™ CA-9 Instant Adhesive One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.A slower setting version of CA-.. |
|||
Viscosity | 1000 cP | 1000 cP | "A" component |
ACC QGel 310 QSI Quantum Silicones High Strength Gel QGel 310 is a clear, very soft, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provid.. |
|||
Viscosity | <= 1000 cP @Temperature 75.0 °C |
<= 1000 cP @Temperature 167 °F |
|
Aquabond Technologies Aquabond™ ABS-55 Water Soluble Adhesive and Bonding Thermoplastic Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem.. |
|||
Viscosity | 1000 - 2500 cP | 1000 - 2500 cP | |
Aremco Graphi-Coat™ 623 High Temperature Specialty Coatings Inorganic, Titanium Diboride Filled This coating system, originally patented by Aremco, is a tow-part, silica-bonded, titanium diboride filled, oxidation resistant coating for protecting graphite from oxidation to 2000°F (1093°C). U.. |
|||
Viscosity | 1000 cP | 1000 cP | |
BASF Lupranate® 5060 Isocyanate Description: Lupranate® 5060 Isocyanate is a low functional prepolymer based on monomeric MDI. Lupranate® 5060 isocyanate is suitable for use in a broad range of flexible, semi-flexible, and cast .. |
|||
Viscosity | 1000 - 2000 cP | 1000 - 2000 cP | |
Beijing Ranger Chem SM-601RX65 Solvent Based Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 1000 cP | 1000 cP | Part A |
Resinlab® UR3010 Black Polyurethane Potting System Resinlab™ UR 3010 Black is a, two component, room temperature curing polyurethane potting system. It is designed to cure completely at room temperature. UR 3010 provides excellent environmental pro.. |
|||
Viscosity | <= 1000 cP | <= 1000 cP | RP-0596 |
Solvay RHODAPEX® ES-2/K Surfactant Chemical Name: SODIUM ALKYL ETHOXY SULFATECAS: 68585-34-2Available in: Asia Pacific, Europe, Latin America and North America Applications: RHODAPEX© ES-2/K is an aqueous solution of sodium lauryl e.. |