Latrobe LSSâ„¢ 420 HC High Carbon Stainless Steel

Category Metal , Ferrous Metal , Martensitic , Stainless Steel
Manufacturer Latrobe Steel
Trade Name LSS™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe LSSâ„¢ 420 HC High Carbon Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TLS 420 HC is a high-carbon martensitic stainless steel which exhibits an attainable hardness of approximately 55 HRC and good wear resistance. TLS 420 HC should be considered for applications such as specialty knives, industrial knives, cutlery, rolls, plastic extrusion tooling, scissors, surgical knives, bearings, and other applications which require a combination of corrosion resistance and wear resistance.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Specific Gravity 7.70 g/cc
7.70 g/cc
Density 7.70 g/cc
0.278 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 54
54
Air Cooled from 982°C, 30 minutes
56
56
Air Cooled from 1010°C, 30 minutes
57
57
Air Cooled from 1025°C, 30 minutes
Modulus of Elasticity 207 GPa
30000 ksi
Machinability 50 - 55 %
50 - 55 %
1% Carbon Steel
Izod Impact Unnotched 13.6 J
10.0 ft-lb
Air Cooled from 1010°C; 393°C Temper Temperature
20.3 J
15.0 ft-lb
Air Cooled from 1010°C; 593°C Temper Temperature
Thermal Properties Metric English Comments
CTE, linear 10.5 µm/m-°C

@Temperature 20.0 - 100 °C
5.83 µin/in-°F

@Temperature 68.0 - 212 °F
12.0 µm/m-°C

@Temperature 20.0 - 500 °C
6.67 µin/in-°F

@Temperature 68.0 - 932 °F
Thermal Conductivity 30.0 W/m-K

@Temperature 20.0 °C
208 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
31.11 W/m-K

@Temperature 199 °C
215.9 BTU-in/hr-ft²-°F

@Temperature 390 °F
32.44 W/m-K

@Temperature 399 °C
225.1 BTU-in/hr-ft²-°F

@Temperature 750 °F
Component Elements Properties Metric English Comments
Carbon, C 0.46 %
0.46 %
Chromium, Cr 13 %
13 %
Iron, Fe 85.44 %
85.44 %
Manganese, Mn 0.40 %
0.40 %
Silicon, Si 0.40 %
0.40 %
Vanadium, V 0.30 %
0.30 %
Electrical Properties Metric English Comments
Volume Resistivity 0.0000548 ohm-cm
0.0000548 ohm-cm
Chemical Properties Metric English Comments
Critical Temperature 799 °C
1470 °F
Ac1
860 °C
1580 °F
Ac3