Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Unnotched | 13.6 J | 10.0 ft-lb | Air Cooled from 1010°C; 393°C Temper Temperature |
Latrobe LSSâ„¢ 420 HC High Carbon Stainless Steel TLS 420 HC is a high-carbon martensitic stainless steel which exhibits an attainable hardness of approximately 55 HRC and good wear resistance. TLS 420 HC should be considered for applications such .. |
|||
Izod Impact Unnotched | 13.6 J | 10.0 ft-lb | Air Cooled from 1010°C; 393°C Temper Temperature |
Latrobe LSSâ„¢ 420 MQ Plastic Mold Steel (AISI 420) TLS 420 MQ is a highly-refined, Mold Quality stainless steel that is engineered to exhibit excellent polishability, good corrosion resistance, and good wear resistance. TLS 420 MQ is melted using an.. |
|||
Izod Impact Unnotched | 13.6 J | 10.0 ft-lb | Air Cooled from 1010°C; 393°C Temper Temperature |
Latrobe LSSâ„¢ 420 Supreme Plastic Mold Steel (AISI 420) TLS 420 Supreme is a specially-refined, mold-quality stainless steel that is engineered to provide supreme polishability, good corrosion resistance, and good wear resistance. TLS 420 supreme is manu.. |
|||
Izod Impact Unnotched | 13.6 J | 10.0 ft-lb | Oil Quenched at 1191°C; 510°C Temper Temperature |
Latrobe Dynamax™ ASTM M42, DIN 1.3247 Super High Speed Steel Dynamax super high speed steel is a premium cobalt high speed steel with a chemical composition designed for high hardness and superior hot hardness. These properties make the steel an excellent cho.. |