Mechanical Properties Metric English Comments
Izod Impact Unnotched 20.3 J
15.0 ft-lb
Air Cooled from 1010°C; 593°C Temper Temperature
Latrobe LSSâ„¢ 420 HC High Carbon Stainless Steel
TLS 420 HC is a high-carbon martensitic stainless steel which exhibits an attainable hardness of approximately 55 HRC and good wear resistance. TLS 420 HC should be considered for applications such ..
Izod Impact Unnotched 20.3 J
15.0 ft-lb
Air Cooled from 1010°C; 593°C Temper Temperature
Latrobe LSSâ„¢ 420 MQ Plastic Mold Steel (AISI 420)
TLS 420 MQ is a highly-refined, Mold Quality stainless steel that is engineered to exhibit excellent polishability, good corrosion resistance, and good wear resistance. TLS 420 MQ is melted using an..
Izod Impact Unnotched 20.3 J
15.0 ft-lb
Air Cooled from 1010°C; 593°C Temper Temperature
Latrobe LSSâ„¢ 420 Supreme Plastic Mold Steel (AISI 420)
TLS 420 Supreme is a specially-refined, mold-quality stainless steel that is engineered to provide supreme polishability, good corrosion resistance, and good wear resistance. TLS 420 supreme is manu..
Izod Impact Unnotched 20.3 J
15.0 ft-lb
Oil Quenched from 954°C; As Quenched
Latrobe LSSâ„¢ D3 Tool Steel (ASTM D3)
TLS D3 tool steel is a high-carbon, high-chromium, oil-hardening tool steel that is characterized by a relatively high attainable hardness and numerous, large, chromium-rich alloy carbides in the mi..
Izod Impact Unnotched 20.3 J
15.0 ft-lb
Oil Quenched at 1238°C; 622°C Temper Temperature
Latrobe Dynavanâ„¢ ASTM T15 Super High Speed Steel
DYNAVAN (T15) is a super high speed steel designed for extra-high wear resistance and superior hot hardness. These properties result from the high carbon and vanadium contents which produce numerous..