Thermal Properties Metric English Comments
Thermal Conductivity 30.0 W/m-K

@Temperature 20.0 °C
208 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Latrobe LSSâ„¢ 420 HC High Carbon Stainless Steel
TLS 420 HC is a high-carbon martensitic stainless steel which exhibits an attainable hardness of approximately 55 HRC and good wear resistance. TLS 420 HC should be considered for applications such ..
Thermal Conductivity 30.0 W/m-K

@Temperature 700 °C
208 BTU-in/hr-ft²-°F

@Temperature 1290 °F
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel
W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to ..
Thermal Conductivity 30.0 W/m-K

@Temperature 500 °C
208 BTU-in/hr-ft²-°F

@Temperature 932 °F
Bohler-Uddeholm BÖHLER W403 VMR® Hot Work Tool Steel
W403 VMR is a modified hot work alloy with an excellent combination of hot tensile properties and toughness. The balanced properties of this grade are not only due to chemistry modification, but to ..
Thermal Conductivity 30.0 W/m-K

@Temperature 199 °C
208 BTU-in/hr-ft²-°F

@Temperature 390 °F
hardened to 57 HRC
Bohler-Uddeholm COMPAX™ AISI S7 MOLD QUALITY Cold Work Steel
Chromium-molybdenum alloyed steelA versatile S7 grade recommended for applications demanding a high degree of toughness and moderate wear resistance. Successfully used for heavy-duty punching and sh..
Thermal Conductivity 30.0 W/m-K

@Temperature 599 °C
208 BTU-in/hr-ft²-°F

@Temperature 1110 °F
hardness of 45 HRC
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel
Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o..
Thermal Conductivity 30.0 W/m-K

@Temperature 599 °C
208 BTU-in/hr-ft²-°F

@Temperature 1110 °F
hardness of 45 HRC
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel
Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o..
Thermal Conductivity 30.0 W/m-K

@Temperature 199 °C
208 BTU-in/hr-ft²-°F

@Temperature 390 °F
hardened to 60 HRC
Bohler-Uddeholm UDDEHOLM VANADIS 4 EXTRA® Powder Metallurgically Produced Tool Steel
Description: Uddeholm Vanadis 4 Extra is a chromiummolybdenum-vanadium alloyed steel Vanadis 4 Extra is characterized by: Very good ductility High abrasive-adhesive wear resistance High compressive..
Thermal Conductivity 30.0 W/m-K

@Temperature 399 °C
208 BTU-in/hr-ft²-°F

@Temperature 750 °F
hardened to 60 HRC
Bohler-Uddeholm UDDEHOLM VANADIS 4 EXTRA® Powder Metallurgically Produced Tool Steel
Description: Uddeholm Vanadis 4 Extra is a chromiummolybdenum-vanadium alloyed steel Vanadis 4 Extra is characterized by: Very good ductility High abrasive-adhesive wear resistance High compressive..
Thermal Conductivity 30.0 W/m-K

@Temperature 100 °C
208 BTU-in/hr-ft²-°F

@Temperature 212 °F
American Utility Metals Cromgard® Stainless Steel
Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o..
Thermal Conductivity 30.0 W/m-K

@Temperature 800 °C
208 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Assab Steels QRO 90 SUPREME Hot Work Steel
QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista..
Thermal Conductivity 30.0 W/m-K

@Temperature 204 °C
208 BTU-in/hr-ft²-°F

@Temperature 400 °F
Schmolz + Bickenbach Cryodur® 2357(S-7) Cold Work Die Steel
Description: Cryodur 2357 is a shock resistant tool steel with excellent toughness and high strength; Suitable for cold and hot work applications up to 1000 °F; and Supplied in the annealed conditi..