Chemical Properties | Metric | English | Comments |
---|---|---|---|
Critical Temperature | 799 °C | 1470 °F | Ac1 |
Latrobe LSSâ„¢ 420 HC High Carbon Stainless Steel TLS 420 HC is a high-carbon martensitic stainless steel which exhibits an attainable hardness of approximately 55 HRC and good wear resistance. TLS 420 HC should be considered for applications such .. |