Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 32.44 W/m-K @Temperature 399 °C |
225.1 BTU-in/hr-ft²-°F @Temperature 750 °F |
|
Latrobe LSSâ„¢ 420 HC High Carbon Stainless Steel TLS 420 HC is a high-carbon martensitic stainless steel which exhibits an attainable hardness of approximately 55 HRC and good wear resistance. TLS 420 HC should be considered for applications such .. |