Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LTL Color Compounds ColorRxâ„¢ PE2-0202AF Food Grade HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer LTL Color Compounds
Trade Name ColorRx™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF LTL Color Compounds ColorRxâ„¢ PE2-0202AF Food Grade HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color Compounders, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.945 g/cc
0.945 g/cc
ASTM D792
Melt Flow 0.60 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
0.60 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ASTM D1238
2.0 g/10 min
<br>@Load 5.00 kg,<br> Temperature 190 °C
2.0 g/10 min
<br>@Load 11.0 lb,<br> Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Modulus 0.951 GPa
138 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 68.9 °C
156 °F
(0.250&quot;); ASTM D648