Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 68.9 °C
156 °F
(0.250"); ASTM D648
LTL Color Compounds ColorRxâ„¢ PE2-0200RX Biocompatible HDPE
A biocompatiblei fractional melt High Density Polyethylene for healthcare applicationsAll information provided by LTL Color Compounders, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 68.9 °C
156 °F
(0.250"); ASTM D648
LTL Color Compounds ColorRxâ„¢ PE2-0201A Antimicrobial HDPE
A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color ..
Deflection Temperature at 0.46 MPa (66 psi) 68.9 °C
156 °F
(0.250"); ASTM D648
LTL Color Compounds ColorRxâ„¢ PE2-0202AF Food Grade HDPE
A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color ..
Deflection Temperature at 0.46 MPa (66 psi) 68.9 °C
156 °F
(0.250"); ASTM D648
LTL Color Compounds ColorRxâ„¢ PE2-0202ARX Biocompatible, Antimicrobial HDPE
A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color ..
Deflection Temperature at 0.46 MPa (66 psi) 68.9 °C
156 °F
(0.250"); ASTM D648
LTL Color Compounds ColorRxâ„¢ PE2-0205ARX Biocompatible, Antimicrobial HDPE
A biocompatible fractional melt High Density Polyethylene for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided ..
Deflection Temperature at 0.46 MPa (66 psi) 68.9 °C
156 °F
ISO 75-2/B
ExxonMobil Exxtral™ BNU 013 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good impact resistance, high stiffness, good scratch and good surface finishing designed for automotive interior ap..
Deflection Temperature at 0.46 MPa (66 psi) 68.9 °C
156 °F
ASTM D648
ExxonMobil HDPE HD 6605.70 High Density Polyethylene Copolymer Resin
Product Description: HD 6605.70 is a narrow molecular weight hexane copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balan..
Deflection Temperature at 0.46 MPa (66 psi) 68.9 °C
156 °F
Molded and tested in accordance with ASTM D4976; ASTM D648
Dow DMDA-8965 NT 7 High Density Polyethylene Resin
DOW DMDA-8965 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as food containers. Information provided by Dow
Deflection Temperature at 0.46 MPa (66 psi) 68.9 - 142 °C
156 - 288 °F
Average value: 104 °C Grade Count:30