Polymer Property : Flexural Modulus = 0.951 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.951 GPa
138 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Network Polymers NPP 25-2002
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Flexural Modulus 0.951 GPa
138 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Network Polymers NPP 25-2003
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
Flexural Modulus 0.951 GPa
138 ksi
ASTM D790
LTL Color Compounds ColorRxâ„¢ PE2-0200RX Biocompatible HDPE
A biocompatiblei fractional melt High Density Polyethylene for healthcare applicationsAll information provided by LTL Color Compounders, Inc.
Flexural Modulus 0.951 GPa
138 ksi
ASTM D790
LTL Color Compounds ColorRxâ„¢ PE2-0201A Antimicrobial HDPE
A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color ..
Flexural Modulus 0.951 GPa
138 ksi
ASTM D790
LTL Color Compounds ColorRxâ„¢ PE2-0202AF Food Grade HDPE
A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color ..
Flexural Modulus 0.951 GPa
138 ksi
ASTM D790
LTL Color Compounds ColorRxâ„¢ PE2-0202ARX Biocompatible, Antimicrobial HDPE
A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color ..
Flexural Modulus 0.951 GPa
138 ksi
ASTM D790
LTL Color Compounds ColorRxâ„¢ PE2-0205ARX Biocompatible, Antimicrobial HDPE
A biocompatible fractional melt High Density Polyethylene for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided ..
Flexural Modulus 0.951 GPa
138 ksi
ISO 178
LyondellBasell Hifaxâ„¢ CA387 Thermoplastic Polyolefin Elastomer
Description: Hifax â„¢ CA387 is a thermoplastic polyolefin elastomer suitable for automotive exterior partsFeatures: Good StiffnessGood ProcessabilityGood Impact ResistanceGood Colorability Paint..
Flexural Modulus 0.951 GPa
138 ksi
Secant; ISO 178
ExxonMobil Exxtral™ BNT 013 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior applications such as door panels.Availability: Africa & Middle East, Asia Pacific, E..
Flexural Modulus >= 0.951 GPa
>= 138 ksi
ASTM D790
Buckeye Polymers BP FLEX D5618 T RXF Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist..