Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.60 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.60 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers MS 125 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Melt Flow | 0.60 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.60 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Premix Thermoplastics PRE-ELEC® PP 1386 PRE-ELEC PP 1386 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Melt Flow | 0.60 - 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.60 - 0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 2260M (601F7) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.60 - 0.80 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.60 - 0.80 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6752G (526H7) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.60 - 0.80 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.60 - 0.80 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6845G (446H7) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.60 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.60 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 TPC-ET
(Unverified Data**) Hytrel® HTR8223 BK320 is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 42D, is pigmented black with fine particle size carbon black, a.. |
|||
Melt Flow | 0.60 - 0.80 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.60 - 0.80 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 4222M (224F7) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.60 - 0.80 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.60 - 0.80 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6753G (526H7) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.60 - 0.80 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.60 - 0.80 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6844G (446H7) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.60 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.60 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PE2-0200RX Biocompatible HDPE A biocompatiblei fractional melt High Density Polyethylene for healthcare applicationsAll information provided by LTL Color Compounders, Inc. |
|||
Melt Flow | 0.60 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.60 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PE2-0201A Antimicrobial HDPE A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color .. |
|||
Melt Flow | 0.60 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.60 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PE2-0202AF Food Grade HDPE A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color .. |
|||
Melt Flow | 0.60 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.60 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PE2-0202ARX Biocompatible, Antimicrobial HDPE A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color .. |
|||
Melt Flow | 0.60 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.60 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PE2-0205ARX Biocompatible, Antimicrobial HDPE A biocompatible fractional melt High Density Polyethylene for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided .. |
|||
Melt Flow | <= 0.60 g/10 min @Load 2.16 kg, Temperature 190 °C |
<= 0.60 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
MTM Plastics Purpolen® PE Polyethylene Regrind Purpolen® is a sorted regrind material suited to the production of demanding end user products. Extrusion and injection molding grades are available in many colors. The basis of our Purpolen® .. |
|||
Melt Flow | 0.60 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.60 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133/ASTM D1238 |
Silon Taborex TA 1135 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1135 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Melt Flow | 0.60 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.60 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis BE50-7032 Polypropylene Homopolymer for Non-Pressure pipes and extruded sheets BE50-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer characterized by high stiffness, high heat distortion temperature and high resistance to thermal aging.
The materia.. |
|||
Melt Flow | 0.60 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.60 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HDPE HD 7960..13 High Density Polyethylene Resin Product Description: HD 7960.13 is a high molecular weight HDPE blown film resin. Films made from HD 7960.13 exhibit excellent impact and toughness properties, as well as high stiffness. HD 7960.13 .. |
|||
Melt Flow | 0.60 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.60 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 7500E Description: Extrusion Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.60 g/10 min @Load 5.00 kg, Temperature 200 °C |
0.60 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ABS 9301 Description: Extrusion Grade, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 0.60 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.60 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Eraclene® FA 506 Hexene Copolymer High Density Polyethylene - Blown Film Extrusion Eraclene FA 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.Its broad molecular weight distribution and density successfully c.. |
|||
Melt Flow | 0.60 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.60 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® VL 29 HDPE Extrusion and pipe applications.Information provided by Unipetrol RPA |