Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
Omni Plastics OmniTuff™ HPP CCF40 Homopolymer Polypropylene Calcium Carbonate Filled Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni.. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | 2 in/min; ASTM D638 |
Polimeros Mexicanos Rotolene® ECO-BLACK Linear Medium Density Polyethylene MDPE Copolymer with UV8 stabilizer, available as black powder.Recommended for rotomolding. Used for manufacture of septic tanks and garbage bins. Recommended for use in combination with ROTOFOAM B.. |
|||
Tensile Strength, Yield | 21.4 MPa @Temperature 121 °C |
3100 psi @Temperature 250 °F |
ASTM D638 |
Network Polymers Nylon 0304NL Description: Natural NylonInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
Rochling Engineered Plastics Polystone® Natural (UHMW-PE) Polystone® M is a highly versatile polymer that features: Low coefficient of friction Excellent abrasion resistance High-impact strength Chemical resistance Complies with FDA regulations under the .. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® L64220UT1 Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Large tanks, material handling equipment and industrial rotational molding applications.Formolene L64220U is fully heat and UV stabilized.Meets all requirements of the .. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D 638 |
LyondellBasell Pro-faxâ„¢ SG899 Polypropylene Copolymer Description: Pro-faxâ„¢ SG899 high flow, high impact polypropylene copolymer resin is tailored for use in automotive interior head impact applications. This resin is designed to be run in convent.. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | Type 1 Specimen, Rate: 2"/min; ASTM D638 |
Global GPP-2500 Polypropylene Impact Copolymer, Nucleated Information provided by Global Polymers Corporation. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® PBA2000 PBT/ABS Alloy, Flame Retarded Flame-retarded V0-rated PBT/ABS alloyAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PE2-0200RX Biocompatible HDPE A biocompatiblei fractional melt High Density Polyethylene for healthcare applicationsAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PE2-0201A Antimicrobial HDPE A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color .. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PE2-0202AF Food Grade HDPE A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color .. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PE2-0202ARX Biocompatible, Antimicrobial HDPE A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color .. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
LTL Color Compounds ColorRxâ„¢ PE2-0205ARX Biocompatible, Antimicrobial HDPE A biocompatible fractional melt High Density Polyethylene for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided .. |
|||
Tensile Strength, Yield | 21.4 MPa @Temperature 23.0 °C |
3100 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Polene HI830 Polystyrene APPLICATIONS: EXTRUSION APPLICATION, VACUUM SHEET : FOOD PACKAGING ELECTRICAL APPLIANCES, HOUSEHOLD PRODUCT, TOYS, SANITARY, etc. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
JPJ Technologies PP PE35-1 Impact copolymer for Injection Molding PP M700R is impact copolymer of good fluidity, excellent impact resistance at low temperature, good rigid-tough balance and improves stiffness. Products made from this resin are characterized by fas.. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
Techmer ES Statiblend® 02020 MB Polypropylene, 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 5% Filler by Weight/Unspecified FillerReinforFeatures: ConductiveTPCI# 9117116Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
Techmer ES Statiblend® 02056 BKN Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveAppearance: BlackTPCI# 9109116Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D412 |
Teknor Apex APEX® 3300-90 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, RadiationUses-Automotive Applications, Food Service Applications, General Purpose, Med.. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
Total PPC 5724 Polypropylene, Extra High Impact Copolymer ATOFINA 5724 is characterized by a high fluidity offering a combination of processing and excellent impact properties in applications ranging from industrial to household.ApplicationATOFINA 5724 has.. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D412 |
Clariant OMAN698583 Thermoplastic Polyurethane, Halogen Free, Flame Retardant Aromatic Polyether BasedData provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
Aaron Industries AAROLENE® ARPS 100-3 HIPS Black Injection Grade Polystyrene Compounded Resin, Injection Molding AAROLENE® ARPS 100 Series Polystyrene Compounded ResinFeatures: A high impact Polystyrene, custom colored black, featuring good flow and excellent toughness. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D638 |
Techmer ES Statiblend® PP TM10 BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 10% Filler by WeightFeatures: ConductiveUL File Number: E157318Appearance: BlackInformation provided by TP Composites, Inc.. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | ASTM D-638 |
Axiall 1025-115A Flexible PVC Non-lead stabilized, 85C rated harness compound formulated for SAE J1128 applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 21.4 MPa | 3100 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® L64220U Rotational Molding LLDPE
(discontinued **) Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L64220U is a general-purpose rotational molding linear low density resin made using the BP Gas Phase ProcessTM. Th.. |