Polymer Property : Specific Gravity = 0.945 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.945 g/cc
0.945 g/cc
ASTM D792
Quadrant EPP TIVAR® 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material (ASTM Product Data Sheet)
Specific Gravity 0.945 g/cc
0.945 g/cc
ASTM D792
LTL Color Compounds ColorRxâ„¢ PE2-0200RX Biocompatible HDPE
A biocompatiblei fractional melt High Density Polyethylene for healthcare applicationsAll information provided by LTL Color Compounders, Inc.
Specific Gravity 0.945 g/cc
0.945 g/cc
ASTM D792
LTL Color Compounds ColorRxâ„¢ PE2-0201A Antimicrobial HDPE
A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color ..
Specific Gravity 0.945 g/cc
0.945 g/cc
ASTM D792
LTL Color Compounds ColorRxâ„¢ PE2-0202AF Food Grade HDPE
A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color ..
Specific Gravity 0.945 g/cc
0.945 g/cc
ASTM D792
LTL Color Compounds ColorRxâ„¢ PE2-0202ARX Biocompatible, Antimicrobial HDPE
A fractional melt High Density Polyethylene containing antimicrobial protection. Ingredients are not approved for biocompatibility or food contact applications.All information provided by LTL Color ..
Specific Gravity 0.945 g/cc
0.945 g/cc
ASTM D792
LTL Color Compounds ColorRxâ„¢ PE2-0205ARX Biocompatible, Antimicrobial HDPE
A biocompatible fractional melt High Density Polyethylene for healthcare applications, containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided ..
Specific Gravity 0.945 g/cc
0.945 g/cc
ASTM D1505
SCG Chemicals EL-Leneâ„¢ S10 Butene (C4) Rotational Molding Resin
Color compound resin available in pellet / powder formKey Characteristics:Excellent stiffnessFair impact resistanceFair processingTypical Applications: High-load/High performance products, such as ..
Specific Gravity 0.945 g/cc
0.945 g/cc
ASTM D1505
Chevron Phillips Marlex® C513UV High Density Polyethylene, Blow Molding
This extra high molecular weight, hexane copolymer is tailored for intermediate bulk container applications that require:Outstanding impact resistanceOutstanding ESCRExcellent processabilityUV stabi..
Specific Gravity 0.945 g/cc
0.945 g/cc
Radici Radilene® R 30 IE 0 3036 B Low Density Polyethylene
Shore hardness: 55 D (3s)Processable, recyclable, no charge and completely non-toxicApplication examples: coating of corrugated and non-corrugated pipe (conduit, plumbing pipe, steel pipe coating a..