LTL Color Compounds ColorRxâ„¢ PE2-0200RX Biocompatible HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer LTL Color Compounds
Trade Name ColorRx™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LTL Color Compounds ColorRxâ„¢ PE2-0200RX Biocompatible HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A biocompatiblei fractional melt High Density Polyethylene for healthcare applicationsAll information provided by LTL Color Compounders, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.945 g/cc
0.945 g/cc
ASTM D792
Melt Flow 0.60 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.60 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
2.0 g/10 min

@Load 5.00 kg,
Temperature 190 °C
2.0 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Modulus 0.951 GPa
138 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 68.9 °C
156 °F
(0.250"); ASTM D648