Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical SEETEC M1425 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer LG Chemical
Trade Name SEETEC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical SEETEC M1425 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: SEETEC M1425 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1425 exhibits a very high stiffness and a good impact strength. SEETEC M1425 meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520 for food contact.Applications: Battery Cases, Out door Chairs, Automotive Parts, Housewares CAS No. 9010-79-1Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D1505
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 27.5 MPa
3980 psi
50mm/min; ASTM D638
Elongation at Break >= 200 %
>= 200 %
50mm/min; ASTM D638
Flexural Modulus 1.77 GPa
256 ksi
ASTM D760
Izod Impact, Notched 0.883 J/cm

@Temperature 23.0 °C
1.65 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 130 - 170 °C
266 - 338 °F
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ASTM D648
Vicat Softening Point 155 °C

@Load 1.00 kg
311 °F

@Load 2.20 lb
ASTM D1525
Flash Point >= 340 °C
>= 644 °F
Descriptive Properties Value Comments
Autoignition Temperature >350°C