DuPont Performance Polymers Elvamide® 8063 Nylon  (Unverified Data**)

Category Polymer , Thermoplastic , Nylon
Manufacturer DuPont Performance Polymers
Trade Name Elvamide®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Elvamide® 8063 Nylon  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyamide Multipolymer with Improved Gel Resistance in SolutionsInformation provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
DAM; ASTM D792
Water Absorption at Saturation 3.4 %
3.4 %
DAM; Immersion 24h; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 71
71
DAM; ASTM D785
Tensile Strength 52.0 MPa
7540 psi
DAM; ASTM D638
Descriptive Properties Value Comments
Additives Release agent
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America