High thermal conductivity product based on Polyamide 12 (PA12), impact modified. Special filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 3.00 g/cc
0.108 lb/in³
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cm
0.0070 - 0.010 in/in
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cm
0.0070 - 0.010 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.0 MPa
2180 psi
Elongation at Break 5.0 %
5.0 %
Tensile Modulus 0.900 GPa
131 ksi
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
Thermal Properties Metric English Comments
Thermal Conductivity 2.00 W/m-K
13.9 BTU-in/hr-ft²-°F
Longitudinal
Maximum Service Temperature, Air 80.0 °C
176 °F
Deflection Temperature at 0.46 MPa (66 psi) 55.0 °C
131 °F
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °C
104 °F
Vicat Softening Point 60.0 °C

@Load 5.00 kg
140 °F

@Load 11.0 lb
Processing Properties Metric English Comments
Melt Temperature 240 - 260 °C
464 - 500 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 70.0 - 90.0 °C

@Time 10800 sec
158 - 194 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa