Hong Kun Group UV 234 UV Absorber

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Hong Kun Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hong Kun Group UV 234 UV Absorber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UV 234 is a high molecular weight ultraviolet light absorber (UVA) of the hydroxyl phenyl benzotriazole class, imparting outstanding light stability to polymers usually processed at high temperatures such as polycarbonate, polyesters, polyacetal, polyamides, polyphenylene sulfide, polyphenylene oxide, aromatic copolymers, thermoplastic polyurethane and polyurethane fibers, where loss of UVA is not tolerated as well as for polyvinylchloride, styrene homo- and copolymers. Applications include molded articles, films, sheets and fibers.UV 234 has world wide Food Contact Approvals in most polymers and is especially suitable in packaging applications for food, consumer care products and pharmaceuticals.Chemical Name: 2-(2H-benzotriazol-2-yl)-4,6- bis(1-methyl-1-phenylethyl) phenolCAS No. 70321-86-7All information provided by Hongkun Group
Physical Properties Metric English Comments
Volatiles <= 0.50 %
<= 0.50 %
Molecular Weight 447.6 g/mol
447.6 g/mol
Ash <= 0.10 %
<= 0.10 %
Thermal Properties Metric English Comments
Melting Point 137 - 141 °C
279 - 286 °F
Optical Properties Metric English Comments
Transmission, Visible >= 97 %

@Wavelength 450 nm
>= 97 %

@Wavelength 450 nm
>= 98 %

@Wavelength 500 nm
>= 98 %

@Wavelength 500 nm
Descriptive Properties Value Comments
Appearance light yellow powder/granule
Purity (%) >= 99