Solvay MACKAMIDE® S Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name MACKAMIDE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay MACKAMIDE® S Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Mackamide S is a high molecular weight oil soluble alkanolamide. It can form water in oil emulsions and can be used as a corrosion inhibitor. In personal care applications Mackamide S provides good viscosity performance. In most formulations, Mackamide S provides a modest amount of conditioning as well as imparting the desirable lubricating feel of soap. Mackamide S has a low free diethanolamine content that meets the requirements of the European directive relating to residual diethanolamine in alkanolamides used in personal care products. INCI Name: Soyamide DEA CAS: 68603-38-3 EINECS: 271-653-9 Uses: Shampoo, Hand Soap, Body Wash, Foam Booster/Stabilizer, Liquid Dishwash, Emulsifier and Corrosion InhibitionInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
Optical Properties Metric English Comments
Gardner Color Number <= 6.0
<= 6.0
Processing Properties Metric English Comments
Shelf Life 48.0 Month
48.0 Month
Descriptive Properties Value Comments
Appearance Clear Liquid
Composition DEA
4-7% MW 105
Free DEA
<5.0%, Exclusive Alkalinity due to Soap and Free Catalyst
Free Fatty Acid
<0.2%, MW 282