Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.224 g/cc | 0.00809 lb/in³ | |
Kraton® G1650 M (SEBS) Linear Triblock Copolymer Description: Kraton G1650 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide.. |
|||
Bulk Density | 0.224 - 0.400 g/cc | 0.00810 - 0.0145 lb/in³ | Loose |
KaMin KaMin® 2000C Kaolin Clay - Calcined Highest brightness, smallest particle size, calcined kaolin clay, more cost -effective Ti02 extender than KaMin® 70C.Industry: Paint & CoatingsUses: Architectural Coatings, Industrial Coatings, F.. |
|||
Bulk Density | 0.224 - 0.400 g/cc | 0.00810 - 0.0145 lb/in³ | Loose |
KaMin Polyfil® 90 Kaolin Clay - Calcined Highest brightness, smallest particle size, calcined kaolin.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, Butyl Rubber, General Plastics, Polyolefins/PVC, Thermoset, Thermo.. |
|||
Bulk Density | 0.224 g/cc | 0.00810 lb/in³ | Dry |
Skamol Group SUPER ISOL Calcium Silicate Insulating Slab SKAMOL SUPER calcium silicate slabs have the following characteristics: Max. service temperature: Up to 1100°C (2012°F)Back-up insulation onlyExtremely lightweightVery low thermal conductivity.. |
|||
Bulk Density | 0.224 g/cc | 0.00810 lb/in³ | Loose |
CIMBAR CIMTUFF® 9102 Talc CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® .. |
|||
Bulk Density | 0.224 g/cc | 0.00810 lb/in³ | |
BNZ Materials Zelieblok 1900S Structural Ceramic Insulation Information provided by BNZ Materials Inc. |