Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D412 |
Huntsman IROGRAN® PS 455-215 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
300% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D412 |
Huntsman KRYSTALFLEX® PE 193 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
300% Modulus | 0.00552 GPa | 0.801 ksi | measured on films cast from a solution in toluene; ASTM D412 |
Kraton® D1184 K (SBS) Branched Triblock Copolymer Description: Kraton D1184 K is a clear, branched triblock copolymer based on styrene and butadiene, with a polystyrene content of 31%. It is supplied from North America in the physical form indentif.. |
|||
300% Modulus | 0.00552 GPa | 0.801 ksi | ASTM D412 |
Kraton® G1650 M (SEBS) Linear Triblock Copolymer Description: Kraton G1650 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form ide.. |
|||
300% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D412 |
Huntsman IROGRAN® A 60 E 4612 N TPU-Polyester Performance Features: Manufactures of technical parts can achieve the highest levels of: Wear and tear strengthDimensional stabilityOil resistanceLow compression setDynamic load performanceElasticit.. |
|||
300% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D412-97 |
Saint-Gobain Norprene® A-60-F Food Process Tubing Formulation Description: Norprene® Food Process Tubing, Formulation A-60-F: Formulated to withstand the high temperatures frequently occurring during food and beverage processing, Norprene® Food Process.. |
|||
300% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D412-98 |
Saint-Gobain Norprene® A-60-G Industrial Grade Tubing Formulation Description: Norprene® Industrial Grade Tubing, Formulation A-60-G: Norprene® Industrial Grade Tubing outperforms neoprene, EPDM and other general-purpose tubings in test after test and appl.. |
|||
300% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D412-98 |
Saint-Gobain Tygon® Norprene® A-60-F I.B. Pressure Tubing Formulation for CIP and SIP cleaning and sterilization systems Good for use in clean-in-place and steam-in-place cleaning and sterilization systems, Norprene® Pressure Tubing has excellent alkali resistance and is compatible with numerous oxidizing agents su.. |
|||
300% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2790 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00552 GPa | 0.800 ksi | ASTM D412 |
Lubrizol Estane® ALR E72A Thermoplastic Polyurethane Type: Estane® ALR E72A is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor.. |