Material Notes:
NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impact strength, excellent chemical and hydrolytic resistance, higher thermal performance, excellent clarity, recyclable & non-toxic, low flammabilityInformation provided by US distributor, API-Kolon.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
DIN 53479; ASTM D792
Water Absorption 0.070 %
0.070 %
DIN 53475; ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Melt Flow 16 g/10 min

@Temperature 275 °C
16 g/10 min

@Temperature 527 °F
DSC
Mechanical Properties Metric English Comments
Hardness, Rockwell R 88
88
DIN 53505; ASTM D785
Tensile Strength, Ultimate 58.8 MPa
8530 psi
DIN 53455; ASTM D638
Elongation at Break 400 %
400 %
DIN 53455; ASTM D638
Flexural Yield Strength 89.2 MPa
12900 psi
DIN 53455; ASTM D790
Flexural Modulus 2.73 GPa
395 ksi
DIN 53452; ASTM D790
Izod Impact, Notched 0.490 J/cm
0.918 ft-lb/in
DIN 53453; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 60 µm/m-°C

@Temperature 20.0 °C
33 µin/in-°F

@Temperature 68.0 °F
DIN 53752; ASTM D696
Melting Point 241 °C
466 °F
DIN 53736; ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ASTM D648
Glass Transition Temp, Tg 82.0 °C
180 °F
DSC
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
ASTM D1003