Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.73 GPa | 396 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging PK8-1080 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LUX1619 PC Lexan* LUX1619 Polycarbonate resin is an extrusion grade. It is UL94 HB rated. It was designed for high light reflectance. |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LUX2619 PC Lexan* LUX2619 Polycarbonate resin is an extrusion grade. It is UL94 V-2 rated at 1.5 mm. It was designed for high light reflectance. |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Lexan® LUX2619 PC (Europe-Africa-Middle East) Lexan* LUX2619 Polycarbonate resin is an extrusion grade. It is UL94 V-2 rated at 1.5 mm. It was designed for high light reflectance. |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | ASTM D790 |
PolyOne Geon™ CPVC EC050 Polyvinyl Chloride, Chlorinated (CPVC) The Geon EC050 CPVC is an extrusion compound for Industrial Pipe applications where enhanced resistance at elevated temperatures is needed. Geon EC050 demonstrates ease of processing and excellent t.. |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | ASTM D790 |
PolyOne Geon™ CPVC EC950 Polyvinyl Chloride, Chlorinated (CPVC) The Geon EC950 CPVC is an extrusion compound for Industrial Pipe applications where enhanced resistance at elevated temperatures is needed. It is listed under NSF Std 14 and 61. Geon EC950 demonstra.. |
|||
Flexural Modulus | 2.73 GPa | 395 ksi | DIN 53452; ASTM D790 |
Kolon NOPLA® KE531 PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 1-3120 B DEL 20% Talc Filled Polypropylene Homopolymer INNOPOL® CS 1-3120 B DEL is developed for producing injection molded automotive components.All information provided by INNO-COMP. |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX05305C PC (Asia Pacific) LNP* Stat-kon* DX05305C is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP AF001H ABS LNP* THERMOCOMP* AF001H is a compound based on ABS resin containing 5% Glass Fiber. Added feature of this material is: Healthcare. |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DX05305C PC LNP* STAT-KON* DX05305C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP AF001H ABS (Asia Pacific) LNP* Thermocomp* AF001H is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL EXNL1117 PPE+HIPS high gloss Noryl |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS high gloss Noryl |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS (Asia Pacific) high gloss Noryl |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS (Europe-Africa-Middle East) high gloss Noryl |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | ASTM Test |
BASF Ultramid® 8260 40% Mineral Filled PA6 (Conditioned) Ultramid 8260 is a 40% mineral reinforced PA6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability including low.. |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | ASTM D-790 |
Axiall 7055 Rigid PVC, Extrusion Georgia Gulf 7055 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: WeatherabilityChemicalDurabilityEase of ProcessingToughnessInformat.. |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | ASTM D790 |
PolyOne Geon™ CPVC LC500 Polyvinyl Chloride, Chlorinated (CPVC) Geon LC500 CPVC is an extrusion grade rigid compound. It is designed for applications where enhanced resistance at elevated temperatures is needed. LC500 demonstrates ease of processing with excelle.. |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | ASTM D-790 |
Axiall 7055 Rigid PVC, Extrusion, White Georgia Gulf 7055 White is a special purpose rigid PVC extrusion compound designed for window and door applications. The compound exhibits the following characteristics: WeatherabilityChemical Res.. |
|||
Flexural Modulus | 2.73 GPa | 396 ksi | ASTM D790 |
Polimeri Europa SINKRAL G523 ABS, High Impact
(discontinued **) High impact; good flow; high gloss.Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line. |