Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Ultimate = 58.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 58.8 MPa
8530 psi
DIN 53455; ASTM D638
Kolon SPESIN® KP210 General Purpose PBT Resin  (discontinued **)
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea..
Tensile Strength, Ultimate 58.8 - 81.4 MPa
8530 - 11800 psi
Average value: 68.7 MPa Grade Count:6
Overview of materials for PEN-PET
This property data is a summary of similar materials in the MatWeb database for the category "PEN-PET". Each property range of values reported is minimum and maximum values of appropriate MatWeb ent..
Tensile Strength, Ultimate 58.8 MPa
8530 psi
ASTM D638
Kolon Kocetal® TC704 Reinforced Grade Acetal Copolymer  (Unverified Data**)
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Tensile Strength, Ultimate 58.8 MPa
8530 psi
ASTM D638
Kolon Kocetal® EC701 Modified Grade Acetal Copolymer  (discontinued **)
Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ..
Tensile Strength, Ultimate 58.8 MPa
8530 psi
DIN 53455; ASTM D638
Kolon KOPA® KN173HI2 High Impact Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Tensile Strength, Ultimate 58.8 MPa
8530 psi
DIN 53455; ASTM D638
Kolon NOPLA® KE531 PEN-PET Copolyester
NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac..
Tensile Strength, Ultimate 58.8 MPa
8530 psi
DIN 53455; ASTM D638
Kolon SPESIN® KP211 General Purpose PBT Resin
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High..
Tensile Strength, Ultimate 58.8 MPa
8530 psi
ASTM D638
SK Chemicals SKYTHANE® U1753C Ink Binder
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Tensile Strength, Ultimate 58.8 MPa
8530 psi
ASTM D1708
Daelim H&L Plavis-MS DF MoS2 Filled Aromatic Polyimide Bearing
Direct Formed. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is the criti..
Tensile Strength, Ultimate 58.8 MPa
8530 psi
5mm/min; ASTM D638
Asia International Enterprise (Hong Kong) 60T4 Nylon 66, 20% Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.