Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 58.8 MPa | 8530 psi | DIN 53455; ASTM D638 |
Kolon SPESIN® KP210 General Purpose PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Tensile Strength, Ultimate | 58.8 - 81.4 MPa | 8530 - 11800 psi | Average value: 68.7 MPa Grade Count:6 |
Overview of materials for PEN-PET This property data is a summary of similar materials in the MatWeb database for the category "PEN-PET". Each property range of values reported is minimum and maximum values of appropriate MatWeb ent.. |
|||
Tensile Strength, Ultimate | 58.8 MPa | 8530 psi | ASTM D638 |
Kolon Kocetal® TC704 Reinforced Grade Acetal Copolymer
(Unverified Data**) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Tensile Strength, Ultimate | 58.8 MPa | 8530 psi | ASTM D638 |
Kolon Kocetal® EC701 Modified Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Tensile Strength, Ultimate | 58.8 MPa | 8530 psi | DIN 53455; ASTM D638 |
Kolon KOPA® KN173HI2 High Impact Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Tensile Strength, Ultimate | 58.8 MPa | 8530 psi | DIN 53455; ASTM D638 |
Kolon NOPLA® KE531 PEN-PET Copolyester NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac.. |
|||
Tensile Strength, Ultimate | 58.8 MPa | 8530 psi | DIN 53455; ASTM D638 |
Kolon SPESIN® KP211 General Purpose PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Tensile Strength, Ultimate | 58.8 MPa | 8530 psi | ASTM D638 |
SK Chemicals SKYTHANE® U1753C Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Tensile Strength, Ultimate | 58.8 MPa | 8530 psi | ASTM D1708 |
Daelim H&L Plavis-MS DF MoS2 Filled Aromatic Polyimide Bearing Direct Formed. Plavis-MS: MoS2 15 wt% filled, Self lubricating grade for vacuum environments.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded to 3 carbons is the criti.. |
|||
Tensile Strength, Ultimate | 58.8 MPa | 8530 psi | 5mm/min; ASTM D638 |
Asia International Enterprise (Hong Kong) 60T4 Nylon 66, 20% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |