Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kolon KOCETAL® UR302 Toughened Grade Acetal Resin

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Impact Modified
Manufacturer Kolon
Trade Name Kocetal®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon KOCETAL® UR302 Toughened Grade Acetal Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TPU added, improved toughness. Applications: Impact resistant, flexible products. Information provided by API-Kolon
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
ASTM D955
Melt Flow 10 - 13 g/10 min
10 - 13 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 75
75
ASTM D785
Tensile Strength 44.0 MPa
6380 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Strength 64.0 MPa
9280 psi
ASTM D790
Flexural Modulus 1.96 GPa
284 ksi
ASTM D790
Izod Impact, Notched 0.490 J/cm
0.918 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 166 °C
331 °F
ASTM D1525
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257
Users viewing this material also viewed the following: