Polymer Property : Tensile Strength = 44.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 44.0 MPa
6380 psi
ASTM D638
Kolon KOCETAL® MS301 Wear Modified Acetal Resin
Molybdenum disulfide added, improved wear property. Applications: Products for low noise and friction against metal. Information provided by API-Kolon.
Tensile Strength 44.0 MPa
6380 psi
ASTM D638
Kolon KOCETAL® SO301 Wear Modified Acetal Resin
Silicone Oil added, improved wear property. Information provided by API-Kolon.
Tensile Strength 44.0 MPa
6380 psi
ASTM D638
Kolon KOCETAL® TC704 Mineral Reinforced Acetal Resin
Whisker reinforced, improved wear and dimensional property. Applications: Dimensionally precise products. Information provided by API-Kolon.
Tensile Strength 44.0 MPa
6380 psi
ASTM D638
Kolon KOCETAL® UR302 Toughened Grade Acetal Resin
TPU added, improved toughness. Applications: Impact resistant, flexible products. Information provided by API-Kolon
Tensile Strength 44.0 MPa
6380 psi
ASTM D412
GRECO ISOTHANE 3055D Polyether TPU Resin
ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod..
Tensile Strength 44.0 MPa
6380 psi
DIN 53455
Isoflon PA 12 Polyamide 12
General use for mechanical partsGood heat resistanceEasy to useInformation provided by Isoflon.
Tensile Strength >= 44.0 MPa
>= 6380 psi
ISO 37
Austin Novel Materials Texalan® 398A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tensile Strength 44.0 MPa
6380 psi
ISO 527-3/5/500
Lubrizol Estane® 54601 Thermoplastic Polyurethane
Feature: Produces high coating weight in one pass at high production speed. Broad process window and transparent spherical pellets.Uses: Melt roll coated fabrics and unsupported foilsAvailable in A..
Tensile Strength 44.0 MPa
6380 psi
DIN 53455
Isoflon PA 11 Polyamide 11
General use for mechanical partsGood heat resistanceEasy to useInformation provided by Isoflon.