Kolon KOCETAL® GF302 G/F Reinforced Acetal Resin

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, 10% Glass Fiber Reinforced
Manufacturer Kolon
Trade Name Kocetal®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kolon KOCETAL® GF302 G/F Reinforced Acetal Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass fiber reinforced, improved stiffness. Applications: Products for high stiffness, improved fatigue properties.Information provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
Ash 8.0 - 12 %
8.0 - 12 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 85
85
ASTM D785
Tensile Strength 94.0 MPa
13600 psi
ASTM D638
Elongation at Break 10.3 %
10.3 %
ASTM D638
Flexural Strength 142 MPa
20600 psi
ASTM D790
Flexural Modulus 4.745 GPa
688.2 ksi
ASTM D790
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 166 °C
331 °F
ASTM D1525
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
ASTM D257