Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.48 g/cc | 1.48 g/cc | 23/23°C; ASTM D792 |
RheTech Products FRG130-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Flame Retardant, Black Applications: Electrical component housingsSunroof componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
PolyOne Nymax™ GMF 600 A 40 HS Natural Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
PolyOne Nymax™ GMF 604 40 UV Black 28 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R1700E Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
PolyOne Geon™ Vinyl Flexible R8570A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
LG Chemical LUMID LW4403B(W) PA66+GF/MF40%, Low Warpage Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
KYDEX® 6503 Integral Pearlescent Low Heat Release Aviation Thermoforming Sheet Features:Thicknesses from 0.71 mm to 3.18 mmChemical resistant - easy to clean with aggressive cleanersForms deep draws with low forces when heated to the upper end of forming temperature rangeCrisp.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ISO 1183 |
Lanxess Pocan® B 3233 HR 000000 Polybutylene Terephthalate, 30% Glass Fibers PBT, 30% glass fibers, injection molding, improved flowability, hydrolysis stabilized |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
Lucent Polymers L6-140 Nylon 6, 15% Glass Fiber and 25% Mineral Reinforced Add "H" for Heat Stabilized Add "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | |
Sylvin Technologies 9950-95 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | |
Sylvin Technologies 9960-90 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON EEF42 PEI LNP STAT-KON* EEF42 is a compound based on Polyetherimide resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
SPS Guang Zhou POBUXâ„¢ 3001EPG15 Non-halogen flame retardance/GF15%-PBT Characteristic: Good flame retardance, high mechanical properties, high rigidity, superior heat resistance, good dimensional stabilityApplications: E/E partsInformation Provided by SPS (Guang Zhou) .. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® TK-6036H PPA, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
Teknor Apex Sinvicomp SSG 5003 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Good Flexibility Uses: Cable Jacketing; Wire and Cable Applications Wire Types: ST4; ST5; TM1; YM1; YM2 Agency Ratings: BS 6746; IEC 60227; VDE 0207 Forms: Pell.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | |
TSE Industries Thanecure® T9 Polyfunctional Isocyanate Additive Thanecure T9 is a polyfunctional isocyanate which is used as a vulcanization agent for polyurethane rubbers and as an adhesion promoter for rubber to textile bonding. Thanecure T9 is used as a vulca.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Poly White P80494PF Concentrate Based In Polypropylene DescriptionPOLYBATCH® P80494PF is a color matched white color concentrate based in polypropylene. This concentrate was designed to provide opacity and color polypropylene film, extrusion, and mold.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Blue 4300 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 4300 is a blue color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 4.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White P8555 SC Concentrate Based In Random Copolymer Polypropylene DescriptionPOLYBATCH® P8555 SC is a high quality white masterbatch containing 50% TiO2 based in random copolymer polypropylene. This product offers excellent dispersion and a very low moisture con.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White P8555 SC Concentrate Based In Random Copolymer Polypropylene DescriptionPOLYBATCH® P8555 SC is a high quality white masterbatch containing 50% TiO2 based in random copolymer polypropylene. This product offers excellent dispersion and a very low moisture con.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Bright White P80514PF Concentrate Based In Polypropylene DescriptionPOLYBATCH® P80514PF is a bright white color concentrate based in polypropylene. This concentrate was designed to provide opacity and color in polypropylene film, extrusion, and molding .. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Poly White P80494PF Concentrate Based In Polypropylene DescriptionPOLYBATCH® P80494PF is a color matched white color concentrate based in polypropylene. This concentrate was designed to provide opacity and color polypropylene film, extrusion, and mold.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White P8555 SD Concentrate Based In Homopolymer Polypropylene DescriptionPOLYBATCH® P8555 SD is a white masterbatch containing 50% TiO2 based in homopolymer polypropylene. This product offers excellent dispersion and a very low moisture content which permits.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ White P80754PF Concentrate Based In Polypropylene DescriptionPOLYBATCH® P80754PF is a color matched white color concentrate based in polypropylene. This concentrate was designed to provide opacity and color in polypropylene film, extrusion, and m.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ISO 1183 |
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, Conditioned Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ISO 1183 |
Ascend Performance Materials Vydyne® R220/R228 Nylon 66, 40% Mineral Reinforced, Conditioned (2.5% Moisture) Vydyne® R220 is a 40% mineral reinforced Nylon 66 resin formulated for improved impact strength. Also available in black as R228. It is an injection molding grade formulated to retain the inherent .. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | ASTM D792 |
Bayshore Vinyl Compounds BVC 7200-65 Vinyl Compound BVC 7200-65 is an economy grade flexible vinyl formulation designed for easy processing and excellent heat stability. This material will process at high rates with low temperatures and produces a s.. |
|||
Specific Gravity | 1.48 g/cc | 1.48 g/cc | Dry; ASTM D792 |
Asahi Kasei Leona® CR301 Nylon 66 Suitable for a switch insulator. Low abrasion and superior electrical properties.Applications:Sliding switch insulators Information provided by Asahi Kasei |