Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.745 GPa | 688.2 ksi | ASTM D790 |
Kolon KOCETAL® GF302 G/F Reinforced Acetal Resin Glass fiber reinforced, improved stiffness. Applications: Products for high stiffness, improved fatigue properties.Information provided by API-Kolon. |