Polymer Property : Flexural Modulus = 688.2 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.745 GPa
688.2 ksi
ASTM D790
Kolon KOCETAL® GF302 G/F Reinforced Acetal Resin
Glass fiber reinforced, improved stiffness. Applications: Products for high stiffness, improved fatigue properties.Information provided by API-Kolon.