Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

JPJ Technologies PP C120 PP Copolymer Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer JPJ Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF JPJ Technologies PP C120 PP Copolymer Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by JPJ Technologies
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.5 MPa
4280 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
1% Secant Modulus 1500 MPa
218000 psi
ASTM D790A
Izod Impact, Notched (ISO) 9.50 kJ/m²
4.52 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 108 °C
226 °F
ASTM D648