PolyOne Maxxam™ FR PE 161 HDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Maxxam™ FR PE 161 HDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V-0, and 5VA performance ratings. In addition, many compounds in the Maxxam FR portfolio offer elevated Relative Thermal Index (RTI) ratings.*HARDNESS DATA IS BASED ON SINGLE LOT DATA.
Physical Properties Metric English Comments
Specific Gravity 0.998 g/cc
0.998 g/cc
ASTM D792
Melt Flow 0.91 - 2.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.91 - 2.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
65

@Time 10.0 sec
65

@Time 0.00278 hour
ASTM D2240
Tensile Strength, Yield 20.7 MPa
3000 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 500 %
500 %
Type I, 51 mm/min; ASTM D638
Gardner Impact 21.5 J

@Thickness 3.18 mm,
Temperature 23.0 °C
15.9 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 67.0 °C

@Thickness 3.18 mm
153 °F

@Thickness 0.125 in
Annealed; ASTM D648
Flammability, UL94 V-2

@Thickness 0.750 mm
V-2

@Thickness 0.0295 in
NC; UL 94
Oxygen Index 27 %

@Thickness 3.18 mm
27 %

@Thickness 0.125 in
ASTM D2863
Descriptive Properties Value Comments
Features Flame Retardant
Forms Pellets
Generic Name Polyethylene, High Density (HDPE)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant