Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus | 1500 MPa | 218000 psi | ASTM D790A |
JPJ Technologies PP C120 PP Copolymer Injection Molding Information provided by JPJ Technologies |
|||
1% Secant Modulus | 1500 MPa | 218000 psi | ASTM D790A |
JPJ Technologies PP H35S Homopolymer for Injection Molding PP H35S is specifically developed for producing injection molding articles for general purpose applications. It gives consistent processability and high gloss in the products. Application: General u.. |