Azoty Tarnow™ TARFLEN SM-S15 PTFE

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Manufacturer Azoty Tarnow™ (Zaklady Azotowe)
Trade Name TARFLEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Azoty Tarnow™ TARFLEN SM-S15 PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
15% glass fiber reinforced for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Physical Properties Metric English Comments
Density 2.21 g/cc
0.0798 lb/in³
ISO 1183
Filler Content 15 %
15 %
Glass Fibers
Particle Size 40 µm
40 µm
Average
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ISO 868
Ball Indentation Hardness 33.0 MPa
4790 psi
ISO 2039-1
Tensile Strength, Yield 18.0 MPa
2610 psi
ISO 527
Elongation at Break 260 %
260 %
ISO 527
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ISO 180
Thermal Properties Metric English Comments
CTE, linear 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ASTM E 831
Melting Point 327 °C
621 °F
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Processing Temperature 370 °C
698 °F
Molding
Back Pressure 30.0 - 45.0 MPa
4350 - 6530 psi
Molding Pressure